Art and Engineering

Fatigue Calculator

Endurance limit modifiers and Goodman/Soderberg.

Fatigue safety factor (Goodman)
1.699
Corrected endurance limit
201.7 MPa
All results and steps ↓

Material

MPa
MPa

Marin factors

mm

Stresses

MPa
MPa

Diagram

mean stress σₘalternating σₐoperating point (n = 1.7)SₑSᵤₜSᵧ— Goodman- - Gerber- - Soderberg··· Langer (yield)

Results

Fatigue safety factor (Goodman)
1.699
Corrected endurance limit
201.7MPa
First-cycle yield factor (Langer)
2.65
Gerber safety factor
2.108
Soderberg safety factor
1.605
ASME-elliptic safety factor
2.19
Uncorrected endurance limitSₑ′
312.5MPa
Surface factorkₐ
0.819
Size factork_b
0.8787
Load factork_c
1
Reliability factorkₑ
0.897

Calculation steps

  1. 1Rotating-beam endurance limit
    Sₑ′ = 0.5·Sᵤₜ (Sᵤₜ ≤ 1400 MPa)
    Sᵤₜ = 625 MPa
    Sₑ′ = 312.5 MPa
  2. 2Surface factor
    kₐ = a·Sᵤₜ^b
    a = 4.51, b = -0.265 (Sᵤₜ in MPa)
    kₐ = 0.819
  3. 3Size factor
    k_b = 1.24·d^−0.107 (2.79 ≤ d ≤ 51 mm)
    d = 25 mm
    k_b = 0.8787
  4. 4Corrected endurance limit
    Sₑ = kₐ·k_b·k_c·k_d·kₑ·Sₑ′
    Sₑ = 201.7 MPa
  5. 5Modified Goodman
    1/n = σₐ/Sₑ + σₘ/Sᵤₜ
    σₐ = 80 MPa, σₘ = 120 MPa
    n = 1.7
  6. 6Langer first-cycle yield
    n_y = Sᵧ/(σₐ + σₘ)
    n_y = 2.65
Assumptions & limitations
  • Infinite-life design for steels using Marin factors; stresses already include fatigue stress-concentration factor K_f.
  • Uniaxial stress state (or von Mises equivalent alternating and mean stresses).
Limitations
  • Finite-life (S–N) analysis, variable-amplitude loading (Miner's rule) and non-ferrous materials without an endurance limit are not covered.
  • Marin factor fits are empirical; use test data for critical parts.

Results are for general reference. Verify critical dimensions and values before cutting, machining, printing or relying on them for safety.